Process operation of new dry rotary kiln with uneven material

In normal production, the raw material feeding amount is micro-microwave moving, sometimes the equipment will have some problems, or affected by the rainy season, the raw material moisture will change, and the raw material will be agglomerated, resulting in poor material feeding.

Process operation of new dry rotary kiln with uneven material

In normal production, the raw material feeding amount is micro-microwave moving, sometimes the equipment will havesome problems, or affected by the rainy season, the raw material moisture will change, and the raw material will be agglomerated, resulting in poor materialfeeding. The fluctuations are relatively large. In this case, the operator isrequired to observe and adjust frequently, and also has certain predictabilityand make measures in advance. Reduce the impact on production, quality andequipment.

When there is less material, it isforbidden to extend the coal injection pipe, open the exhaust air, and lengthenthe flame. This will cause the temperature of the kiln tail to rise sharply, andthe temperature of the decomposition furnace and the cyclone will rise rapidly,resulting in a cyclone. The tube or the blanking pipe is bonded or evenblocked. The kiln tail chamber and the decomposition furnace are also easy tocrust, which increases the resistance of the system. At this time, the coalinjection pipe should be appropriately removed, the small exhaust gas should beshut off, the coal supply volume of the decomposition furnace and the kiln headshould be reduced, and the kiln tail should be controlled. The temperature andthe temperature of the cyclone are short-burned and the material is returned tonormal.

When there is more incoming material, therewill be positive pressure in the rotary kiln head. The temperature of thecyclone outlet and the decomposition furnace and the temperature of the kilntail will drop sharply. At this time, the kiln speed should be reducedappropriately, the feeding amount should be reduced, and the exhaust air shouldbe opened. Injecting the coal pipe, which can increase the temperature of thekiln tail and enhance the pre-burning effect. At this time, coal can be addedappropriately, but it is not easy to be excessive. If it is considered that itis wrong to add more coal at this time, it will cause a reducing atmosphere andlower the temperature in the kiln. When the material is used for a long time,there is also a lot of exhaust gas, which does not increase the temperature.When the current of the main motor of the kiln drops rapidly, the speed of thekiln is lowered, the coal pipe is withdrawn, and the air volume isappropriately adjusted. At this time, the short flame is used to make it returnto normal. When the working conditions in the kiln are normal, the feeding iscarried out.